| Units English | SI |
| General | ||||
| Material Status |
| |||
| Availability |
| |||
| Features |
| |||
| Uses |
| |||
| Forms |
| |||
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
| Specific Gravity | 1.06 | ASTM D792 | |
| Molding Shrinkage - Flow | 0.015 to 0.025 | in/in | ASTM D955 |
| Hardness | Nominal Value | Unit | Test Method |
| Durometer Hardness (Shore A) | 90 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
| Tensile Stress | ASTM D412 | ||
100% Strain | 1130 | psi | |
300% Strain | 3280 | psi | |
| Tensile Strength (Yield) | 4700 | psi | ASTM D412 |
| Tensile Elongation (Break) | 350 | % | ASTM D412 |
| Tear Strength (Split) | 55 | lbf/in | ASTM D470 |
| Compression Set (158°F) | 65 | % | ASTM D395 |
| Clash-Berg Modulus (75°F) | 10.4 | psi | ASTM D1043 |
| Thermal | Nominal Value | Unit | Test Method |
| Brittleness Temperature | -76.0 | °F | ASTM D746 |
| Electrical | Nominal Value | Unit | Test Method |
| Volume Resistivity | 5.1E+13 | ohm·cm | ASTM D257 |
| Dielectric Strength | 850 | V/mil | ASTM D149 |
| Dielectric Constant | ASTM D150 | ||
100 Hz | 6.00 | ||
100 kHz | 5.30 | ||
| Dissipation Factor | ASTM D150 | ||
100 Hz | 0.025 | ||
100 kHz | 0.042 |
| Thermoset | Nominal Value | Unit | |
| Thermoset Components | |||
Hardener | Mix Ratio by Weight: 11 | ||
Resin | Mix Ratio by Weight: 100 | ||
| Pot Life (212°F) | 4.0 to 6.0 | min | |
| Demold Time (212°F) | 60 to 960 | min |